Design of high entropy alloys based on the experience from commercial superalloys

Download (0 kB)
Version 2 2015-04-14, 12:50
Version 1 2015-01-02, 00:00
journal contribution
posted on 2015-04-14, 12:50 authored by Z. Wang, Y. Huang, J. Wang, C.T. Liu

High entropy alloys (HEAs) have been drawing increasing attention recently and gratifying results have been obtained. However, the existing metallurgic rules of HEAs could not provide specific information of selecting candidate alloys for structural applications. Our brief survey reveals that many commercial superalloys have medium and even to high configurational entropies. The experience of commercial superalloys provides a clue for helping us in the development of HEAs for structural applications.